Adhesion, migration and mechanics of human adipose-tissue-derived stem cells on silk fibroin-chitosan matrix.
Altman AM., Gupta V., Ríos CN., Alt EU., Mathur AB.
Laboratory Study, published in Acta Biomater (2009) — summary generated from the PubMed abstract.
Evidence from laboratory and animal studies provides groundwork for understanding mechanisms and potential before human studies continue.
- Level A · Stronger Clinical Evidence
- Level B · Emerging clinical evidence with positive signals
- Level C · Early human research exploring benefits
- Level D · Scientific groundwork from lab and animal studies
- Emerging · Emerging topic under active research
This page is generated from the PubMed record. The Thai description is an automated summary of bibliographic fields and the abstract, not a full translation, and is not medical advice.
- Study type
- Laboratory Study
- Journal
- Acta Biomater (2009)
- Country
- England
- Reported sample size
- —
- Source database
- PubMed
- PMID
- 19861180
- DOI
- 10.1016/j.actbio.2009.10.034
- Citations
- 29
Abstract (original English)
Silk fibroin-chitosan (SFCS) scaffold is a naturally derived biocompatible matrix with potential reconstructive surgical applications. In this study, human adipose-derived mesenchymal stem cells (ASCs) were seeded on SFCS scaffolds and cell attachment was characterized by fluorescence, confocal, time-lapse, atomic force, and scanning electron microscopy (SEM) studies. Adhesion of ASCs on SFCS was 39.4 + or - 4.8% at 15 min, increasing to 92.8+/-1.5% at 120 min. ASC adhered at regions of architectural complexity and infiltrate into three-dimensional scaffold. Time-lapse confocal studies indicated a mean ASC speed on SFCS of 18.47+/-2.7 microm h(-1) and a mean persistence time of 41.4 + or - 9.3 min over a 2.75 h study period. Cytokinetic and SEM studies demonstrated ASC-ASC interaction via microvillus extensions. The apparent elastic modulus was significantly higher (p<0.0001) for ASCs seeded on SFCS (69.0 + or - 9.0 kPa) than on glass (6.1 + or - 0.4 kPa). Also, cytoskeleton F-actin fiber density was higher (p<0.05) for ASC seeded on SFCS (0.42 + or - 0.02 fibers microm(-1)) than on glass-seeded controls (0.24 + or - 0.03 fibers microm(-1)). Hence, SFCS scaffold facilitates mesenchymal stem cell attachment, migration, three-dimensional infiltration, and cell-cell interaction. This study showed the potential use of SFCS as a local carrier for autologous stem cells for reconstruc
What this study does not prove
- • This study does not prove SVF is an approved treatment or a replacement for standard care.
- • This is preclinical work; animal or laboratory results cannot be applied to humans.
Evidence level
Evidence from laboratory and animal studies provides groundwork for understanding mechanisms and potential before human studies continue.
How we grade evidenceBrowse all related research
Filter the research library by this study's title keywords, author, or publication year.