Level D· Scientific groundwork from lab and animal studiesAnimal StudyPubMed

Bone tissue engineering by using a combination of polymer/Bioglass composites with human adipose-derived stem cells.

Lu W., Ji K., Kirkham J., Yan Y., Boccaccini AR., Kellett M.

Animal Study, published in Cell Tissue Res (2014) — summary generated from the PubMed abstract.

Open my reading list
Level D· Scientific groundwork from lab and animal studiesEvidence level of this study

Evidence from laboratory and animal studies provides groundwork for understanding mechanisms and potential before human studies continue.

  • Level A · Stronger Clinical Evidence
  • Level B · Emerging clinical evidence with positive signals
  • Level C · Early human research exploring benefits
  • Level D · Scientific groundwork from lab and animal studies
  • Emerging · Emerging topic under active research
Read the A–D evidence level guide

This page is generated from the PubMed record. The Thai description is an automated summary of bibliographic fields and the abstract, not a full translation, and is not medical advice.

Study type
Animal Study
Journal
Cell Tissue Res (2014)
Country
Germany
Reported sample size
—
Source database
PubMed
PMID
24408074
DOI
10.1007/s00441-013-1770-z
Citations
30

Abstract (original English)

Translational research in bone tissue engineering is essential for "bench to bedside" patient benefit. However, the ideal combination of stem cells and biomaterial scaffolds for bone repair/regeneration is still unclear. The aim of this study is to investigate the osteogenic capacity of a combination of poly(DL-lactic acid) (PDLLA) porous foams containing 5 wt% and 40 wt% of Bioglass particles with human adipose-derived stem cells (ADSCs) in vitro and in vivo. Live/dead fluorescent markers, confocal microscopy and scanning electron microscopy showed that PDLLA/Bioglass porous scaffolds supported ADSC attachment, growth and osteogenic differentiation, as confirmed by enhanced alkaline phosphatase (ALP) activity. Higher Bioglass content of the PDLLA foams increased ALP activity compared with the PDLLA only group. Extracellular matrix deposition after 8 weeks in the in vitro cultures was evident by Alcian blue/Sirius red staining. In vivo bone formation was assessed by using scaffold/ADSC constructs in diffusion chambers transplanted intraperitoneally into nude mice and recovered after 8 weeks. Histological and immunohistochemical assays indicated significant new bone formation in the 40 wt% and 5 wt% Bioglass constructs compared with the PDLLA only group. Thus, the combination of a well-developed biodegradable bioactive porous PDLLA/Bioglass composite scaffold with a high-potenti

What this study does not prove

  • • This study does not prove SVF is an approved treatment or a replacement for standard care.
  • • This is preclinical work; animal or laboratory results cannot be applied to humans.

Evidence level

Evidence from laboratory and animal studies provides groundwork for understanding mechanisms and potential before human studies continue.

How we grade evidence
Adipose TissueAlkaline PhosphataseAnimalsBone and BonesCell AdhesionCell ProliferationCell SurvivalCeramicsCollagenHumans

Browse all related research

Filter the research library by this study's title keywords, author, or publication year.