Level D· Scientific groundwork from lab and animal studiesLaboratory StudyPubMed

Characterization of zinc-releasing three-dimensional bioactive glass scaffolds and their effect on human adipose stem cell proliferation and osteogenic differentiation.

Haimi S., Gorianc G., Moimas L., Lindroos B., Huhtala H., Räty S.

Laboratory Study, published in Acta Biomater (2009) — summary generated from the PubMed abstract.

Open my reading list
Level D· Scientific groundwork from lab and animal studiesEvidence level of this study

Evidence from laboratory and animal studies provides groundwork for understanding mechanisms and potential before human studies continue.

  • Level A · Stronger Clinical Evidence
  • Level B · Emerging clinical evidence with positive signals
  • Level C · Early human research exploring benefits
  • Level D · Scientific groundwork from lab and animal studies
  • Emerging · Emerging topic under active research
Read the A–D evidence level guide

This page is generated from the PubMed record. The Thai description is an automated summary of bibliographic fields and the abstract, not a full translation, and is not medical advice.

Study type
Laboratory Study
Journal
Acta Biomater (2009)
Country
England
Reported sample size
—
Source database
PubMed
PMID
19428318
DOI
10.1016/j.actbio.2009.04.006
Citations
58

Abstract (original English)

While the addition of zinc ions to bioactive ceramics has been shown to enhance the proliferation and osteogenic differentiation of osteoblast-like cells, contradictory results have been found. Therefore, the effect of zinc-releasing ceramics on cell proliferation and differentiation into osteogenic lineages requires further clarification. The aim of this study was to evaluate the effects of zinc addition on the degradation profile of three-dimensional bioactive glass scaffold, and on the proliferation and osteogenesis of human adipose stem cells (hASCs) in these scaffolds. Bioactive glass scaffolds containing Na(2)O, K(2)O, MgO, CaO, B(2)O(3), TiO(2), P(2)O(5) and SiO(2) were prepared. The degradation was evaluated by weight loss measurement, scanning electron microscopy and elemental analysis. The degradation profile of bioactive glass was shown to slow down with the addition of zinc. Qualitative live/dead staining showed that zinc addition to bioactive glass inhibits cell spreading and proliferation of hASCs. However, zinc addition had no significant effect on DNA content, alkaline phosphatase activity and osteopontin concentration of hASCs when measured quantitatively. Our results suggest that the possible stimulatory effect of addition of zinc on hASC proliferation and osteogenesis was not detected because addition of zinc slowed down the degradation rate of the studied bi

What this study does not prove

  • • This study does not prove SVF is an approved treatment or a replacement for standard care.
  • • This is preclinical work; animal or laboratory results cannot be applied to humans.

Evidence level

Evidence from laboratory and animal studies provides groundwork for understanding mechanisms and potential before human studies continue.

How we grade evidence
AdipocytesBone SubstitutesCell Culture TechniquesCell DifferentiationCell ProliferationCells, CulturedFemaleGlassHumansMale

Browse all related research

Filter the research library by this study's title keywords, author, or publication year.