Level D· Scientific groundwork from lab and animal studiesLaboratory StudyPubMed

Electromagnetic field-mediated chitosan/gelatin/nano-hydroxyapatite and bone-derived scaffolds regulate the osteoblastic and chondrogenic phenotypes of adipose-derived stem cells to construct osteochondral tissue enginee

Hu X., Su Y., Xu J., Cheng YY., Liu T., Li X.

Laboratory Study on Cartilage Damage, published in Int J Biol Macromol (2023) — summary generated from the PubMed abstract.

Open my reading list
Level D· Scientific groundwork from lab and animal studiesEvidence level of this study

Evidence from laboratory and animal studies provides groundwork for understanding mechanisms and potential before human studies continue.

  • Level A · Stronger Clinical Evidence
  • Level B · Emerging clinical evidence with positive signals
  • Level C · Early human research exploring benefits
  • Level D · Scientific groundwork from lab and animal studies
  • Emerging · Emerging topic under active research
Read the A–D evidence level guide

This page is generated from the PubMed record. The Thai description is an automated summary of bibliographic fields and the abstract, not a full translation, and is not medical advice.

Study type
Laboratory Study
Journal
Int J Biol Macromol (2023)
Country
Netherlands
Reported sample size
—
Source database
PubMed
PMID
38128807
DOI
10.1016/j.ijbiomac.2023.128829
Citations
8

Abstract (original English)

It is critical to explore the effects of electromagnetic field (EMF) on the construction of functional osteochondral tissue, which has shown certain clinical significance for the treatment of osteochondral injury. At present, there are few studies on the effect of the direction of EMF on cells. This study aimed to investigate the effects of EMF coupling on different parameters to control adipose-derived stem cells (ADSCs) proliferation and specific chondrogenic and osteogenic differentiation at 2D level and 3D level. The proliferation and differentiation of EMF-induced ADSCs are jointly regulated by EMF and space structure. In this study, Cs 7 /Gel 3 /nHAP scaffolds were prepared with good degradation rate (86.75 ± 4.96 %) and absorb water (1100 %), and the pore size was 195.63 ± 54.72 μm. The bone-derived scaffold with a pore size of 267.17 ± 129.18 μm was obtained and its main component was hydroxyapatite. Cs 7 /Gel 3 /nHAP scaffolds and bone-derived scaffolds are suitable as 3D level materials. The optimal EMF intensity was 2 mT for chondrogenic differentiation and proliferation and 1 mT for osteogenic differentiation and proliferation. It is noteworthy that EMF has a negative correlation with ADSCs proliferation in the vertical direction at 2D level, while it has a positive correlation with ADSCs proliferation at 3D level. EMF mediated 3D osteochondral scaffold provide good

What this study does not prove

  • • This study does not prove SVF is an approved treatment or a replacement for standard care.
  • • This is preclinical work; animal or laboratory results cannot be applied to humans.

Evidence level

Evidence from laboratory and animal studies provides groundwork for understanding mechanisms and potential before human studies continue.

How we grade evidence
Tissue EngineeringChitosanDurapatiteOsteogenesisGelatinElectromagnetic FieldsAdipose TissueCell DifferentiationPhenotypeStem Cells