Level D· Scientific groundwork from lab and animal studiesAnimal StudyPubMed

Ethanol-mediated compaction and cross-linking enhance mechanical properties and degradation resistance while maintaining cytocompatibility of a nucleus pulposus scaffold.

Walters JD., Gill SS., Mercuri JJ.

Animal Study on Disc Degeneration, published in J Biomed Mater Res B Appl Biomater (2019) — summary generated from the PubMed abstract.

Open my reading list
Level D· Scientific groundwork from lab and animal studiesEvidence level of this study

Evidence from laboratory and animal studies provides groundwork for understanding mechanisms and potential before human studies continue.

  • Level A · Stronger Clinical Evidence
  • Level B · Emerging clinical evidence with positive signals
  • Level C · Early human research exploring benefits
  • Level D · Scientific groundwork from lab and animal studies
  • Emerging · Emerging topic under active research
Read the A–D evidence level guide

This page is generated from the PubMed record. The Thai description is an automated summary of bibliographic fields and the abstract, not a full translation, and is not medical advice.

Study type
Animal Study
Journal
J Biomed Mater Res B Appl Biomater (2019)
Country
United States
Reported sample size
—
Source database
PubMed
PMID
30767383
DOI
10.1002/jbm.b.34339

Abstract (original English)

Intervertebral disc degeneration is a complex, cell-mediated process originating in the nucleus pulposus (NP) and is associated with extracellular matrix catabolism leading to disc height loss and impaired spine kinematics. Previously, we developed an acellular bovine NP (ABNP) for NP replacement that emulated human NP matrix composition and supported cell seeding; however, its mechanical properties were lower than those reported for human NP. To address this, we investigated ethanol-mediated compaction and cross-linking to enhance the ABNP's dynamic mechanical properties and degradation resistance while maintaining its cytocompatibility. First, volumetric and mechanical effects of compaction only were confirmed by evaluating scaffolds after various immersion times in buffered 28% ethanol. It was found that compaction reached equilibrium at ~30% compaction after 45 min, and dynamic mechanical properties significantly increased 2-6× after 120 min of submersion. This was incorporated into a cross-linking treatment, through which scaffolds were subjected to 120 min precompaction in buffered 28% ethanol prior to carbodiimide cross-linking. Their dynamic mechanical properties were evaluated before and after accelerated degradation by ADAMTS-5 or MMP-13. Cytocompatibility was determined by seeding stem cells onto scaffolds and evaluating viability through metabolic activity and fluor

What this study does not prove

  • • This study does not prove SVF is an approved treatment or a replacement for standard care.
  • • This is preclinical work; animal or laboratory results cannot be applied to humans.

Evidence level

Evidence from laboratory and animal studies provides groundwork for understanding mechanisms and potential before human studies continue.

How we grade evidence
Adipose TissueAnimalsCattleEthanolHumansMaterials TestingNucleus PulposusStem CellsTissue Scaffolds

Browse all related research

Filter the research library by this study's title keywords, author, or publication year.

Related research