NiFe 2 O 4 /ZnO-coated Poly(L-Lactide) nanofibrous scaffold enhances osteogenic differentiation of human mesenchymal stem cells.
Shariati S., Seyedjafari E., Mahdavi FS., Maali A., Ferdosi-Shahandashti E.
Laboratory Study, published in Front Bioeng Biotechnol (2022) — summary generated from the PubMed abstract.
Evidence from laboratory and animal studies provides groundwork for understanding mechanisms and potential before human studies continue.
- Level A · Stronger Clinical Evidence
- Level B · Emerging clinical evidence with positive signals
- Level C · Early human research exploring benefits
- Level D · Scientific groundwork from lab and animal studies
- Emerging · Emerging topic under active research
This page is generated from the PubMed record. The Thai description is an automated summary of bibliographic fields and the abstract, not a full translation, and is not medical advice.
- Study type
- Laboratory Study
- Journal
- Front Bioeng Biotechnol (2022)
- Country
- Switzerland
- Reported sample size
- —
- Source database
- PubMed
- PMID
- 36324893
- DOI
- 10.3389/fbioe.2022.1005028
Abstract (original English)
Background: A combination of bioceramics and polymeric materials has attracted the research community's interest in bone tissue engineering. These composites are essential to support cell attachment, proliferation, and osteogenesis differentiation, which are vital as a classic strategy in bone tissue engineering. In this study, NiFe2O4/ZnO-coated poly L-Lactide (PLLA) was employed as a scaffold to evaluate the osteogenic differentiation capability of human adipose tissue derived mesenchymal stem cells (hAMSCs). Material and methods: The electrospun PLLA nanofibers were fabricated, coated with nanocomposite (NiFe2O4/ZnO), and evaluated by the water contact angle (WCA), tensile test, attenuated total reflectance fourier-transform infrared (ATR-FTIR) and scanning electron microscopy (SEM). Then, the osteogenic differentiation potential of hAMSCs was assessed using NiFe2O4/ZnO-coated PLLA compared to tissue culture plastic (TCP) and a simple scaffold (PLLA) in vitro conditions. Results: The adhesion, proliferation, and differentiation of hAMSCs were supported by the mechanical and biological properties of the NiFe2O4/ZnO-coated PLLA scaffold, according to SEM and 4',6-Diamidino-2-phenylindole dihydrochloride (DAPI) staining patterns. During bone differentiation, Alkaline phosphatase (ALP) enzyme activity, biomineralization, calcium content, and osteogenic gene expression (ALP, Oste
What this study does not prove
- • This study does not prove SVF is an approved treatment or a replacement for standard care.
- • This is preclinical work; animal or laboratory results cannot be applied to humans.
Evidence level
Evidence from laboratory and animal studies provides groundwork for understanding mechanisms and potential before human studies continue.
How we grade evidenceBrowse all related research
Filter the research library by this study's title keywords, author, or publication year.