Level D· Scientific groundwork from lab and animal studiesAnimal StudyPubMed

The stimulation of adipose-derived stem cell differentiation and mineralization by ordered rod-like fluorapatite coatings.

Liu J., Wang X., Jin Q., Jin T., Chang S., Zhang Z.

Animal Study on Face & Skin, published in Biomaterials (2012) — summary generated from the PubMed abstract.

Open my reading list
Level D· Scientific groundwork from lab and animal studiesEvidence level of this study

Evidence from laboratory and animal studies provides groundwork for understanding mechanisms and potential before human studies continue.

  • Level A · Stronger Clinical Evidence
  • Level B · Emerging clinical evidence with positive signals
  • Level C · Early human research exploring benefits
  • Level D · Scientific groundwork from lab and animal studies
  • Emerging · Emerging topic under active research
Read the A–D evidence level guide

This page is generated from the PubMed record. The Thai description is an automated summary of bibliographic fields and the abstract, not a full translation, and is not medical advice.

Study type
Animal Study
Journal
Biomaterials (2012)
Country
Netherlands
Reported sample size
—
Source database
PubMed
PMID
22483243
PMCID
PMC3341557
DOI
10.1016/j.biomaterials.2012.03.050
Citations
30

Abstract (original English)

In this study, the effect of ordered rod-like FA coatings of metal discs on adipose-derived stem cell (ASC)'s growth, differentiation and mineralization was studied in vitro; and their mineral inductive effects in vivo. After 3 and 7 days, the cell number on the metal surfaces was significantly higher than those on the ordered and disordered FA surfaces. However, after 4 weeks much greater amounts of mineral formation was induced on the two FA surfaces with and even without osteogenesis induction. The osteogenic profiles showed the up regulation of a set of pro-osteogenic transcripts and bone mineralization phenotypic markers when the ASCs were grown on FA surfaces compared to metal surfaces at 7 and 21 days. In addition to BMP and TGFβ signaling pathways, EGF and FGF pathways also appeared to be involved in ASC differentiation and mineralization. In vivo studies showed accelerated and enhanced mineralized tissue formation integrated within ordered FA coatings. After 5 weeks, over 80% of the ordered FA coating was integrated with a mineralized tissue layer covering the implants. Both the intrinsic properties of the FA crystals and the topography of the FA coating appeared to dominate the cell differentiation and mineralization process.

What this study does not prove

  • • This study does not prove SVF is an approved treatment or a replacement for standard care.
  • • This is preclinical work; animal or laboratory results cannot be applied to humans.

Evidence level

Evidence from laboratory and animal studies provides groundwork for understanding mechanisms and potential before human studies continue.

How we grade evidence
Adipose TissueAnimalsApatitesBlotting, WesternCalcification, PhysiologicCell AdhesionCell DifferentiationGrowth SubstancesHumansMice

Browse all related research

Filter the research library by this study's title keywords, author, or publication year.

Related research