Level D· Scientific groundwork from lab and animal studiesLaboratory StudyEurope PMCOpen access

Titanium Dioxide Thin Films Obtained by Atomic Layer Deposition Promotes Osteoblasts' Viability and Differentiation Potential While Inhibiting Osteoclast Activity-Potential Application for Osteoporotic Bone Regeneration

Smieszek A., Seweryn A., Marcinkowska K., Sikora M., Lawniczak-Jablonska K., Witkowski BS.

Laboratory Study, published in Materials (Basel) (2020) — summary generated from the PubMed abstract.

Open my reading list
Level D· Scientific groundwork from lab and animal studiesEvidence level of this study

Evidence from laboratory and animal studies provides groundwork for understanding mechanisms and potential before human studies continue.

  • Level A · Stronger Clinical Evidence
  • Level B · Emerging clinical evidence with positive signals
  • Level C · Early human research exploring benefits
  • Level D · Scientific groundwork from lab and animal studies
  • Emerging · Emerging topic under active research
Read the A–D evidence level guide

This page is generated from the PubMed record. The Thai description is an automated summary of bibliographic fields and the abstract, not a full translation, and is not medical advice.

Study type
Laboratory Study
Journal
Materials (Basel) (2020)
Reported sample size
—
Source database
Europe PMC
PMID
33126628
PMCID
PMC7662580
DOI
10.3390/ma13214817
Citations
13

Abstract (original English)

Atomic layer deposition (ALD) technology has started to attract attention as an efficient method for obtaining bioactive, ultrathin oxide coatings. In this study, using ALD, we have created titanium dioxide (TiO 2 ) layers. The coatings were characterised in terms of physicochemical and biological properties. The chemical composition of coatings, as well as thickness, roughness, wettability, was determined using XPS, XRD, XRR. Cytocompatibillity of ALD TiO 2 coatings was accessed applying model of mouse pre-osteoblast cell line MC3T3-E1. The accumulation of transcripts essential for bone metabolism (both mRNA and miRNA) was determined using RT-qPCR. Obtained ALD TiO 2 coatings were characterised as amorphous and homogeneous. Cytocompatibility of the layers was expressed by proper morphology and growth pattern of the osteoblasts, as well as their increased viability, proliferative and metabolic activity. Simultaneously, we observed decreased activity of osteoclasts. Obtained coatings promoted expression of Opn, Coll-1, miR-17 and miR-21 in MC3T3-E1 cells. The results are promising in terms of the potential application of TiO 2 coatings obtained by ALD in the field of orthopaedics, especially in terms of metabolic- and age-related bone diseases, including osteoporosis.

What this study does not prove

  • • This study does not prove SVF is an approved treatment or a replacement for standard care.
  • • This is preclinical work; animal or laboratory results cannot be applied to humans.

Evidence level

Evidence from laboratory and animal studies provides groundwork for understanding mechanisms and potential before human studies continue.