Level D· Scientific groundwork from lab and animal studiesLaboratory StudyPubMed

In vitro biocompatibility of polylactide and polybutylene succinate blends for urethral tissue engineering.

Sartoneva R., Lyyra I., Juusela M., Sharma V., Huhtala H., Massera J.

Laboratory Study, published in J Biomed Mater Res B Appl Biomater (2023) — summary generated from the PubMed abstract.

Open my reading list
Level D· Scientific groundwork from lab and animal studiesEvidence level of this study

Evidence from laboratory and animal studies provides groundwork for understanding mechanisms and potential before human studies continue.

  • Level A · Stronger Clinical Evidence
  • Level B · Emerging clinical evidence with positive signals
  • Level C · Early human research exploring benefits
  • Level D · Scientific groundwork from lab and animal studies
  • Emerging · Emerging topic under active research
Read the A–D evidence level guide

This page is generated from the PubMed record. The Thai description is an automated summary of bibliographic fields and the abstract, not a full translation, and is not medical advice.

Study type
Laboratory Study
Journal
J Biomed Mater Res B Appl Biomater (2023)
Country
United States
Reported sample size
—
Source database
PubMed
PMID
37199480
DOI
10.1002/jbm.b.35268

Abstract (original English)

Surgical treatment of urothelial defects with autologous genital or extragenital tissue grafts is susceptible to complications. Tissue engineering utilizing novel biomaterials and cells such as human urothelial cells (hUC) for epithelial regeneration and adipose stromal cells (hASC) for smooth muscle restoration might offer new treatment options for urothelial defects. Previously, polylactide (PLA) has been studied for urethral tissue engineering, however, as such, it is too stiff and rigid for the application. Blending it with ductile polybutylene succinate (PBSu) could provide suitable mechanical properties for the application. Our aim was to study the morphology, viability and proliferation of hUC and hASC when cultured on 100/0 PLA/PBSu, 75/25 PLA/PBSu blend, 50/50 PLA/PBSu blend, and 0/100 PLA/PBSu discs. The results showed that the hUCs were viable and proliferated on all the studied materials. The hUCs stained pancytokeratin at 7 and 14 days, suggesting maintenance of the urothelial phenotype. The hASCs retained their viability and morphology and proliferated on all the other discs, except on PLA. On the PLA, the hASCs formed large aggregates with each other rather than attached to the material. The early smooth muscle cell markers SM22α and α-SMA were stained in hASC at 7 and 14 day time points on all PBSu-containing materials, indicating that hASCs maintain their smoot

What this study does not prove

  • • This study does not prove SVF is an approved treatment or a replacement for standard care.
  • • This is preclinical work; animal or laboratory results cannot be applied to humans.

Evidence level

Evidence from laboratory and animal studies provides groundwork for understanding mechanisms and potential before human studies continue.

How we grade evidence
HumansTissue EngineeringPolymersPolyestersBiocompatible MaterialsButylene Glycols

Browse all related research

Filter the research library by this study's title keywords, author, or publication year.