Level D· Scientific groundwork from lab and animal studiesAnimal StudyPubMed

Poly(l-Lactic Acid)/Gelatin Fibrous Scaffold Loaded with Simvastatin/Beta-Cyclodextrin-Modified Hydroxyapatite Inclusion Complex for Bone Tissue Regeneration.

Lee JB., Kim JE., Balikov DA., Bae MS., Heo DN., Lee D.

Animal Study on Chronic Wound, published in Macromol Biosci (2016) — summary generated from the PubMed abstract.

Open my reading list
Level D· Scientific groundwork from lab and animal studiesEvidence level of this study

Evidence from laboratory and animal studies provides groundwork for understanding mechanisms and potential before human studies continue.

  • Level A · Stronger Clinical Evidence
  • Level B · Emerging clinical evidence with positive signals
  • Level C · Early human research exploring benefits
  • Level D · Scientific groundwork from lab and animal studies
  • Emerging · Emerging topic under active research
Read the A–D evidence level guide

This page is generated from the PubMed record. The Thai description is an automated summary of bibliographic fields and the abstract, not a full translation, and is not medical advice.

Study type
Animal Study
Journal
Macromol Biosci (2016)
Country
Germany
Reported sample size
—
Source database
PubMed
PMID
26996294
DOI
10.1002/mabi.201500450
Citations
28

Abstract (original English)

Recently, the application of nanostructured materials in the field of tissue engineering has garnered attention to mediate treatment and regeneration of bone defects. In this study, poly(l-lactic acid) (PLLA)/gelatin (PG) fibrous scaffolds are fabricated and β-cyclodextrin (βCD) grafted nano-hydroxyapatite (HAp) is coated onto the fibrous scaffold surface via an interaction between βCD and adamantane. Simvastatin (SIM), which is known to promote osteoblast viability and differentiation, is loaded into the remaining βCD. The specimen morphologies are characterized by scanning electron microscopy. The release profile of SIM from the drug loaded scaffold is also evaluated. In vitro proliferation and osteogenic differentiation of human adipose derived stem cells on SIM/HAp coated PG composite scaffolds is characterized by alkaline phosphatase (ALP) activity, mineralization (Alizarin Red S staining), and real time Polymerase chain reaction (PCR). The scaffolds are then implanted into rabbit calvarial defects and analyzed by microcomputed tomography for bone formation after four and eight weeks. These results demonstrate that SIM loaded PLLA/gelatin/HAp-(βCD) scaffolds promote significantly higher ALP activity, mineralization, osteogenic gene expression, and bone regeneration than control scaffolds. This suggests the potential application of this material toward bone tissue engineeri

What this study does not prove

  • • This study does not prove SVF is an approved treatment or a replacement for standard care.
  • • This is preclinical work; animal or laboratory results cannot be applied to humans.

Evidence level

Evidence from laboratory and animal studies provides groundwork for understanding mechanisms and potential before human studies continue.

How we grade evidence
AnimalsBone DevelopmentCell DifferentiationDurapatiteGelatinHumansOsteogenesisPolyestersRabbitsSimvastatin